Tensile test at room temperature with M5 cladding, hydrogenated to 350 wppm at 800°C in Ar-H2 gas mixture during 4 min (charging from outer side)
Ring compression test at room temperature with M5 cladding, hydrogenated to 2100 wppm at 800°C in Ar-H2 gas mixture during 8 min (charging from inner and outer side)